  • Treatment of defects in post finishing cloth surface

  • 1. The treatment of wool head is caused by the poor cotton yarn distribution and the poor pretreatment of the dyeing plant


    A. semifinished products can be redone slightly, and it is very serious to light the hair and then make mercerization.


    B. finished fabric should be stripped, and then brush, mercerized and colored.


    After C. finished washing to do not consider hair feather, washing can remove or reduce.


    Two, the processing method of the winding phenomenon of elastic fabric